MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BEC Materials SEPS 4030
Categories: Polymer; Thermoplastic

Material Notes: Description: SEPS 4030 has characteristics of fast sol, thickening and anti-shearing performance. Radial structure, Multi-Arm Polymers. Styrene Content, 9% (mass fraction). Appearance, white powder or fluffy granule.

Application: Modified lubricating oil

Formula: Modified lubricating oil
150SN base oil, Sinopec: 90
SEPS YH-4030: 10

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity >= 400 cPToluene solution, 15%
Kinematic Viscosity 10.78 cStafter shearing by Diesel nozzle, Formula
Kinematic Viscosity at 40°C (104°F) 80.13 cStFormula
Kinematic Viscosity at 100°C (212°F) 12.2 cStFormula
 
Chemical PropertiesOriginal ValueComments
Styrene Content 9.0 %Bound
 
Thermal PropertiesOriginal ValueComments
Pour Point -13.0 °CFormula
 
Descriptive Properties
Thickening ability6 mm2/s
 7.04Formula

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBECM091 / 307044

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.