MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance when compared to other ferritic materials such as Type 409, Type 430, and Type 439. This material is resistant to stress corrosion cracking in the presence of chlorides and has excellent formability. This material is ideally suited to automotive exhaust applications where high temperatures or resistance to chlorides in a wet corrosive environment is needed.

CORROSION RESISTANCE AK Steel’s 436L ULTRA FORM® exhibits superior corrosion resistance in synthetic muffler condensate testing when compared to Type 409, Type 430 and Type 439.

OXIDATION RESISTANCE Type 436L ULTRA FORM® is more resistant to high temperature oxidation than Type 409. This is especially true for temperatures exceeding 1500F (816C).

WELDABILITY This stabilized ferritic class of stainless steel is generally considered to be weldable by the common fusion and resistance techniques. To avoid brittle weldments, low weld heat input is recomended. When a weld filler is required, AWS E/ER such as 309 or 330 is often specified.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 74 - 85
Tensile Strength, Ultimate 441 - 517 MPa
Tensile Strength, Yield 276 - 345 MPa
@Strain 0.2 %
Elongation at Break 28 - 35 %in 2 inches
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 17.3 %
Iron, Fe 80.49 %As Remainder
Manganese, Mn 0.30 %
Molybdenum, Mo 1.0 %
Nickel, Ni 0.30 %
Silicon, Si 0.30 %
Titanium, Ti 0.30 %
 
Descriptive Properties
Formability, r1.8
n Value0.20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel ASTM A 1011, Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Overview of materials for T 400 Series Stainless Steel
AISI 9255 Steel, normalized at 900°C (1650°F)
AISI 8822H Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, 150°C (300°F) temper
AISI 8740H Steel, normalized 870°C (1600°F)

NAKS142 / 138558

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.