MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Top Polymer Topolymer® 5111-951E TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Production Description: Topolymer®5111-E is a kind of halogen-free flame-retardant compound which made from SEBS, PE, It was designed specially for parts and cables with requirement of halogen-free flame-retardant.

Features: Excellent flexibility, Good hand feel, Pass the VW-1 standard

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95
Tensile Strength 140 kg(f)/cm²
Elongation at Break 270 %
 
Processing PropertiesOriginal ValueComments
Zone 1 160 - 180 °CExtrusion
Zone 2 190 - 220 °CExtrusion
Zone 3 190 - 220 °CExtrusion
Die Temperature 190 - 230 °CExtrusion
Melt Temperature 200 - 240 °CExtrusion
Head Temperature 190 - 230 °CExtrusion
 
Descriptive Properties
ColorNatural
Compress Ratio2:8:1Extrusion
Filter100-150 MeshExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOPO012 / 184524

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.