MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik REWOQUAT® CPEM Antistatic agent
Categories: Fluid

Material Notes: Product description: Coco pentaethoxy methyl ammonium metho-sulfate

Application: REWOQUAT® CPEM is used as antistatic agent in various textile applications. Besides, it is used as cationic emulsifier or co-emulsifier alone or in combination with non-ionic emulsifiers.

Properties / Benefits: REWOQUAT® CPEM is a highly concentrated, liquid cationic antistatic agent. REWOQUAT® CPEM does not contain any flammable solvent. It is strongly substantive, low-foaming and has emulsifying properties. REWOQUAT® CPEM is compatible with non-ionics, amphoterics and other cationics. With anionic surfactants, REWOQUAT® CPEM usually forms soluble ion pairs. The compatibility of REWOQUAT® CPEM with anionic surfactants has to be checked for each particular case. REWOQUAT® CPEM exhibits good stability versus acids, alkalis, electrolytes and hardness salts in conditions currently encountered in practice. REWOQUAT® CPEM is stable to hydrolysis, has a good heat stability and an outstanding tolerance versus calcium ions. REWOQUAT® CPEM is clearly soluble in cold and warm water up to concentrations of 20 - 30 %. It is soluble in hydrocarbons and chlorinated hydrocarbons at low concentrations (about 5 to 10 %).

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content >= 98 %
pH 5.0 - 7.01% in water
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 12
 
Descriptive Properties
Appearanceyellow, clear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL517 / 196721

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.