Durez® -ter S1063 is a homologous series of hydroxyl terminated polyester diols designed for application in polyurethanes. Durez® -ter S1063 is a fully saturated material based on aliphatic dibasic acid, a carboxylated alcohol and a glycol. Polyesters in this series are liquid, but nevertheless offer excellent performance in urethanes. Availability of this polyester in a broad range of molecular weights permits the formulating chemist great latitude in product development and optimization.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |