MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot foods and drinks when injection molded using conventional chilled molds. Ingeo AW 300D is fully formulated to be used naturally, but may be blended with color compounds.

Information provided by NatureWorks LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Linear Mold Shrinkage 0.003 - 0.006 cm/cm
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 355.3 ksiASTM D790
Izod Impact, Notched 33.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 - 185 °C
Nozzle Temperature 190 - 210 °C
Mold Temperature 25.0 °C
Back Pressure 50.0 - 100 psi
Screw Speed 100 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 3001D Injection Grade PLA
NatureWorks® Ingeo™ 2002D Extrusion Grade PLA
NatureWorks® Ingeo™ 3251D Injection Grade PLA
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware

PNATU73 / 135568

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.