MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 minutes after mixing. It is ideal for many applications requiring a self-extinguishing structural epoxy adhesive system.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 45000 - 90000 cPBase, RVF #7 spindle, 20 rpm
 40000 - 120000 cPAccelerator, RVF #7 spindle, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87ASTM D2240
Modulus of Elasticity 650 ksi
Shear Strength 145 psiOverlap, Polyacrylic
 200 psiOverlap, Polycarbonate
 240 psiOverlap, PVC
 420 psiOverlap, ABS
 600 psiOverlap, FRP
 1050 psiOverlap, Aluminum-MEK/abrade/MEK
 1100 psiOverlap, Cold Rolled Steel-MEK/abrade/MEK
 2100 psiOverlap, after tap water 30 days @ 23°C
 2200 psiOverlap, Aluminum-Etched
 2200 psiOverlap, after 50% RH/RT/30 days
 2700 psiOverlap, after salt spray 30 days @ 23°C
 1250 psi
@Temperature -55.0 °C
Overlap
 2200 psi
@Temperature 23.0 °C
Overlap
 800 psi
@Temperature 82.0 °C,
Time 900 sec
Overlap
Peel Strength 2.00 pli90° T-Peel, Aluminum, etched 2024 T-3; ASTM D1876-61T
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 142 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 20.0 minTime to Handling Strength
 24.0 - 48.0 hour
 
Descriptive Properties
AppearanceCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
Atom Adhesives AA-BOND F112 Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
Dow VORAFORCE™ TW 103/TW 165/TC 3000 Epoxy for Composite Systems
Covestro Makrolon® 1260 Polycarbonate, Impact Grade

PMM34617 / 169364

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.