EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant. Application examples: High strength stretch film, coextrusion, greenhouse film, stretch hood. Information provided by Total Petrochemicals. |