CYCOM® 2020 is a versatile curing, toughened epoxy resin that can be cured from 180°F to 350°F (80°C to 180°C), depending on service temperature requirements. This prepreg resin extracts the maximum possible performance from carbon fibers. The excellent overall balance of properties delivered by CYCOM 2020 has made it the product of choice for many Formula 1 race teams in structural applications. CYCOM 2020 can be either autoclave or vacuum bag cured. Free-standing postcures can also be employed. A one hour cure at 275°F (135°C) gives a Tg of more than 310°F (155°C). The same cure cycle provides excellent mechanical properties with retention of those properties at temperature; 70% of shear strength is retained at 250°F (120°C). CYCOM 2020 is available on both woven and unidirectional carbon, glass and aramid fiber and has a tack-life under ambient conditions in excess of four weeks, maintaining good drape and tack characteristics throughout. Features & Benefits: - Excellent translation of fiber properties
- Excellent retention of mechanical properties at 240°F (120°C) temperature
- High impact resistance
- Controlled flow
- Good drape and tack
- Excellent cured surface finish
- Shop life of 8 weeks at ambient temperature, 75°F (24°C)
Suggested Applications:- High stress extreme performance mast and boom applications
- Structural Formula 1 applications
Property data for CYCOM 2020 T800-6K 5H 280 42% Resin Content 5-Harness Satin Fabric with standard cure (1 hour at 275°F (135°C)).Information provided by Cytec, subsequently acquired by Solvay. |