MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond UV16Med Epoxy Based UV Curable System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Cationic curing, no oxygen inhibition
  • Low shrinkage upon curing
  • Good physical strength properties
  • Passes ISO 10993-5
Product Description: Master Bond UV16Med is a low viscosity, high strength epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is a cationic curing system and has no oxygen inhibition. UV16Med cures quickly when exposed to a UV light source with a wavelength ranging between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of 0.001-0.002 inches up to 0.120 inches, with thinner sections generally curing in 30-60 seconds. Thicker sections will take longer to cure, and post curing with heat will enhance the cured properties. UV16Med bonds well to a wide variety of substrates including plastics, glass and many metals. It is highly resistant to acids, bases, solvents, and numerous sterilants, including ethylene oxide and gluteraldehyde. It also withstands repeated autoclaving. The chemistry of the cured system allows for good thermal cycling capabilities. It is a reliable thermal and electrical insulator with a service temperature range of -80°F to +400°F. Since UV16Med is a cationic curing system, it has a higher glass transition temperature compared to other UV type systems. Post curing with heat is required in achieving a higher Tg. Without heating, the Tg is 90-100°C. If post cured for 30 minutes at 125°C, the Tg increases to about 130-135°C. Additional post curing at this temperature will further increase the Tg allowing for better resistance to autoclaving. UV16Med is an attractive candidate in medical applications where UV light curing is feasible and resistance to sterilization is critical.

Product Advantages:

  • One part system
  • Not oxygen inhibited
  • Outstanding toughness and flexibility
  • Can resist repeated autoclaving
  • Passes ISO 10993-5 for cytotoxicity

Information provided by Master Bond, Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 250 - 500 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70.0 - 80.0
Tensile Strength 7000 - 8000 psi
Tensile Modulus 250000 - 300000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.10
@Frequency 60 Hz
Dissipation Factor 0.0200
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 55.0 µm/m-°C
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -62.0 °C
Glass Transition Temp, Tg 90.0 - 95.0 °Cwithout post cure
 135 - 140 °Cwith post cure
Shrinkage 1.00 - 2.00 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.511
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Monthin original, unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5812 / 323329

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.