MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LG Chemical LP170L PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for synthetic leather foam layer made by Knife coating/ Roll coating/ Gravure coating especially, products made from LP170L are excellent in restoring force and print ability.

Main Applications: Slush molding, synthetic leather, glove

CAS No: 9002-86-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.406 g/cc
Bulk Density 0.290 - 0.390 g/ccASTM D1895
Volatiles <= 1.5 %
@Temperature 110 °C,
Time 3600 sec
ASTM D3030-90
Brookfield Viscosity 2000 - 4000 cPDOP 60phr, 6RPM; ASTM D1824-90
Viscosity Measurement >= 1.0
@Pressure 0.400 MPa
[g/sec], DOP 60phr, Severs; ASTM D1823-90
Molecular Weight 60000 - 150000 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 302 °C
Ignition Temperature 435 °CAutoignition
 
Descriptive Properties
Degree of Polymerization1600-170030°C, JIS K6721-77
K-Value76DIN53726

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omnova Solutions Sunigum® P95 Acrylate Elastomer
Omnova Solutions Chemigum® P83 Nitrile Elastomer
Nitriflex NP-2021 Powdered Nitrile
Mitsubishi Chemical Advanced Materials PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet)
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane

PLAY714 / 148724

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.