MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Medium-leaded brass, 64-1/2%, UNS C34000, OS025, Flat Products, Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Nominal Grain Size 0.025 mm

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Heading and Upsetting; Machining; Piercing and Punching; Roll Threading and Knurling; Stamping

Typical uses: Valve Stems for Tires; Butts; Engravings; Threaded Connectors; Nuts; Rivets; Screws; Couplings; Dials; Flare Fittings; Gears; Instrument Plates; Nuts, Screws Rivets; Screw Machine Products; Drawn Shells; Plumbers' Brass Goods; Plumbing Fittings

Applicable Specifications: Bar – ASTM B121/B121M; Plate - ASTM B121/B121M; Rod, Bar & Shapes – ASTM B453/B453M; Sheet – ASTM B121/B121M; Strip – ASTM B121/B121M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.306 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 ksi
@Thickness 25.4 mm
 50.0 ksi
@Thickness 2.03 mm
 51.0 ksi
@Thickness 1.02 mm
Tensile Strength, Ultimate 34.0 ksi
@Thickness 25.4 mm
In Shear
 34.0 ksi
@Thickness 1.02 mm
In Shear
 34.0 ksi
@Thickness 2.03 mm
In Shear
Tensile Strength, Yield 19.0 ksi
@Thickness 1.02 mm
0.5% Ext
 20.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 50 %
@Thickness 2.03 mm
 53 %
@Thickness 1.02 mm
 60 %
@Thickness 25.4 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 70 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm26% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 67.0 BTU-in/hr-ft²-°F
Melting Point 1630 - 1700 °F
Solidus 1630 °F
Liquidus 1700 °F
Annealing Point 800 - 1200 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 62 - 65 %
Iron, Fe <= 0.15 %
Lead, Pb 0.80 - 1.5 %
Zinc, Zn 33.5 - 37.2 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC34000x4 / 292917

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.