MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa FW-650 Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:
    Features:
  • Weather resistance
  • Super high impact resistance

    Applications:
  • Injection molding
  • Switch
  • Socket

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
@Temperature 23.0 °C
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Temperature 23.0 °C
ASTM D955
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Tensile Strength at Break 37.0 MPa50mm/min; ASTM D638
Elongation at Break 20 %50mm/min; ASTM D638
Flexural Strength 56.0 MPa2mm/min; ASTM D790
Flexural Modulus 2000 MPa2mm/min; ASTM D790
Izod Impact, Notched 287 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 311 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 23.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 91.0 °C
@Load 5.00 kg
50°C/hr; ASTM D1525
 101 °C
@Load 1.00 kg
120°C/hr; ASTM D1525
Flammability Test <= 750[°C]; IEC60695
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 245 °C
Rear Barrel Temperature 180 - 210 °CStart Point: 190°C
Middle Barrel Temperature 190 - 220 °CStart Point: 205°C
Front Barrel Temperature 200 - 230 °CStart Point: 215°C
Melt Temperature 200 - 230 °CStart Point: 220°C
Mold Temperature 30.0 - 60.0 °CStart Point: 50°C
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
Pre-dry
Back Pressure 0.000 - 1.00 MPa
 
Descriptive Properties
Injection SpeedSlow to Moderate
Weather Resistance (delta E)ASTM D4459; 300hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa FW-620 Flame Retardant ABS
Lotte Advanced Materials Starex® NH-0925 S ABS

PKINGF112 / 104371

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.