MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
The Chemical Company Urea
Categories: Other Engineering Material

Material Notes: Urea,CO(NH2)2, is a colorless organic chemical compound compound also known by the International Nonproprietary Name (rINN) carbamide, as established by the World Health Organization. It is highly soluble in water and has a pKa close to zero. Urea is essentially the waste produced when the body metabolizes protein. It is not only produced by humans, but also by many other mammals, as well as amphibians and some fish. Urea was the first natural compound to be artificially synthesized using inorganic compounds.

Information provided by The Chemical Company

Key Words: carbamide;carbonyl diamide;carbonyldiamine
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.750 g/cc
Particle Mesh Size 10 Mesh
pH 7.3 - 9.510% solution
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %
 
Component Elements PropertiesOriginal ValueComments
Nitrogen, N >= 46 %
 
Descriptive Properties
Alkalinity as NH3 (ppm)<120
Angle of Repose34°
AppearanceSolid prills
Assay99%
Biuret (%)< 1.2
Formaldehyde (%)0.2
Hazen Color Value (pt-co)10
Turbidity as SiO2 (ppm)< 20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® 7233 SP 01 TPA
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Melamine-Phenolic Copolymer
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

PTCC012 / 107001

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.