MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ HM612 Glue Sticks - Hot Melt Adhesive
Categories: Polymer; Adhesive

Material Notes: HM612 1/2" x 10" glue sticks are designed for use with the CCH220 Glue Gun for a wide variety of applications. They are clear in color and feature instant tack and fast cure time. It bonds to a variety of metals, concrete, carpet tack strips, Hardie board, plastics, EPDM rubber, foils, and other unique substrates.- Instant tack, 5-minute cure.- Operating temperature of 390° F.- Open time (working time) of 1 minute.- Set time (full cure) of 5 minutes.- Cold / Heat Resistance of -5° F / 135° F.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content <= 0.010 g/l
Viscosity 6000 cP
@Temperature 180 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °F
Softening Point 194 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 356 - 392 °FWorking Temperature
 
Descriptive Properties
Open Time40 sec
Set Time (sec)60
WPS 68 Heat Resistance (g/cm2)100, shear load, @ 130°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI942 / 232153

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.