MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JIS SKH53 Molybdenum High Speed Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Key Words: JIS G4403(83) SKH53, SKH 53, SKH-53; Comparable to AISI M3 Class 2 Tool Steel, UNS T11323
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.16 g/cc(AISI M3 Class 2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 269Bar/Forging Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 - 425 °C
(AISI M3 Class 2)
 12.0 µm/m-°C
@Temperature 20.0 - 540 °C
(AISI M3 Class 2)
 12.8 µm/m-°C
@Temperature 20.0 - 650 °C
(AISI M3 Class 2)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 540 - 595 °CTempering (AISI M3 Class 2)
 1205 - 1230 °CHardening (AISI M3 Class 2)
Annealing Temperature 870 - 900 °C(AISI M3 Class 2)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.1 - 1.3 %
Chromium, Cr 3.8 - 4.5 %
Copper, Cu <= 0.25 %
Iron, Fe 76.7 - 82.2 %As Balance
Manganese, Mn <= 0.40 %
Molybdenum, Mo 4.6 - 6.2 %
Nickel, Ni <= 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.030 %
Tungsten, W 5.5 - 6.7 %
Vanadium, V 2.8 - 3.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
JIS SKH52 Molybdenum High Speed Tool Steel
JIS SKH51 Molybdenum High Speed Tool Steel
Carpenter Micro-Melt® M-4 Alloy (AISI M4)
AISI Type M35 Molybdenum High Speed Tool Steel (UNS T11335)
AISI Type M3 Class 2 Molybdenum High Speed Tool Steel (UNS T11323)

MSTZJSKH53 / 231082

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.