MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M AC-250 B-1/6 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be readily applied with a spatula or extrusion gun. It will cure to a fuel-resistant rubber at temperatures above -6.7°C. It exhibits excellent tooling properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccAMS-S83318
Volatiles 5.0 %
Brookfield Viscosity 900000 - 1.30e+6 cPBase, RVF #6 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40Hydrolytic Stability; AMS-S83318
 55AMS-S83318
Tensile Strength at Break 2.76 MPa
@Time 1.21e+6 sec
Standard Cure; AMS-S83318
 1.38 MPa
@Treatment Temp. 60.0 °C,
Time 1.21e+6 sec
JRF; AMS-S83318
 3.38 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
JRF; AMS-S83318
Elongation at Break 340 %
@Time 1.21e+6 sec
Standard Cure; AMS-S83318
 280 %
@Treatment Temp. 121 °C,
Time 605000 sec
JRF; AMS-S83318
 380 %
@Treatment Temp. 60.0 °C,
Time 1.21e+6 sec
JRF; AMS-S83318
Peel Strength 52.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Alclad; AMS-S83318
 53.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, MIL-C-27725; AMS-S83318
 53.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Alodine; AMS-S83318
 55.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, MIL-C-27725; AMS-S83318
 55.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Stainless Steel; AMS-S83318
 58.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Alclad; AMS-S83318
 60.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Stainless Steel; AMS-S83318
 60.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Titanium; AMS-S83318
 63.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Alodine; AMS-S83318
 65.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Titanium; AMS-S83318
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CAMS-S83318
Minimum Service Temperature, Air -54.0 °CAMS-S83318
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hour
@Temperature 25.0 °C
 10.0 hour
@Temperature 4.40 °C
 14.0 hour
@Temperature -6.70 °C
Tack-Free Time 1.00 hour
@Temperature 25.0 °C
 2.00 hour
@Temperature 4.40 °C
 5.00 hour
@Temperature -6.70 °C
Shelf Life 6.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
AppearanceDark BrownAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Master Bond EP21TPND Two Component Polysulfide Epoxy Adhesive
3M AC-250 A-1/6 Aerospace Sealant
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System
Master Bond EP21TPLV Two Component Epoxy System

PMM35413 / 170160

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.