MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay MIRACARE® SLB-365/G Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Miracare® SLB-365/G is a complete formulated system containing mild anionic and amphoteric foaming surfactants and a structuring agent in an easy to use lamellar concentrate. Upon dilution and processing this performance concentrate can form spherulitic structures which can be used to provide desirable suspension and sensorial properties.

I.N.C.I. Name: WATER, SODIUM TRIDECETH SULFATE, SODIUM LAUROAMPHOACETATE, COCAMIDE MEA, SODIUM CHLORIDE, DMDM HYDANTOIN

CAS: 7732-18-5, 25446-78-0, 68608-66-2, 68140-00-1, 7647-14-5, 6440-58-0

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE© SLB-365/G is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a variety of personal care cleansing products. Typical applications are moisturizing body washes, caring skin cleansers, hair repair shampoos, color protection shampoos, hair moisturizing shampoos, and other type of multi-benefit cleansing formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.10 g/ccRP-17617
Solids Content 48 - 52 %
@Temperature 105 °C,
Time 7200 sec
RP-17628
pH 9.0 - 9.510% Solution; RP-17601
Viscosity <= 5000 cPLVT SP #3, 12 rpm; RP-17619
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0RP-17602
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceHazy, Pourable LiquidRP-0064
CompositionActive38-42%, MW 434, RP-17501
 Free Oil<3.0%, RP-17608
 Glydant0.2-0.3%, RP-17504
 Sodium Chloride<2.5%, RP-17504
 Sodium Sulfate<0.5%, RP-17503
 Total Plate Count<10 cfu/ml, RP-1370
Foreign MatterFree of Foreign Matter

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MIRACARE® SLB-365/N Surfactant
Solvay MIRACARE® SLB-205/N Surfactant

WRHOD251 / 137482

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.