System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Material Notes:
30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.
Information provided by Polyram.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.53
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.10 %
50% RH; ISO 62
Water Absorption at Saturation
0.50 %
ISO 62
Linear Mold Shrinkage
0.0015
-
0.0075
cm/cm
ISO 2577
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
140
MPa
ISO 527
Elongation at Break
3.0 %
ISO 527
Tensile Modulus
9100
MPa
ISO 527
Flexural Strength
200
MPa
ISO 178
Flexural Modulus
8800
MPa
ISO 178
Izod Impact, Notched (ISO)
10.0
kJ/m²
ISO 180
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Dielectric Constant
3.8
IEC 60250
Thermal Properties
Original Value
Comments
Melting Point
225
°C
ISO 11357
Maximum Service Temperature, Air
130
°C
Continuous use
200
°C
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi)
225
°C
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
215
°C
ISO 75
Flammability, UL94
HB
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Envalior Arnite® TV4 261 PBT-GF30, 30% Glass Filled
PPOLYR915 / 126712
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.