MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Marco Polo Mar-Pol ABS GP18 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Processing Method: Injection Molding

Description: General purpose injection molding ABS

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Maximum Moisture Content 0.10
Melt Flow 5.6 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaASTM D638
Tensile Strength, Yield 40.0 MPaASTM D638
Elongation at Break 20 %ASTM D638
Elongation at Yield 2.0 %ASTM D638
Tensile Modulus 2130 MPaASTM D638
Flexural Strength 9860 psiASTM D790
Flexural Modulus 319000 psiASTM D790
Izod Impact, Unnotched 290 J/mASTM D256
Dart Drop, Total Energy 30.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 88.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
CTE, linear, Transverse to Flow 88.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CASTM D648
Vicat Softening Point 98.0 °CASTM D1525
UL RTI, Electrical 60.0 °CUL 746
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °C
Middle Barrel Temperature 205 - 225 °C
Front Barrel Temperature 215 - 240 °C
Nozzle Temperature 220 - 260 °C
Melt Temperature 220 - 260 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 95.0 °C
Dry Time 2.00 - 4.00 hour
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 70 %
Vent Depth 0.0380 - 0.0510 cm
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO013 / 283610

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.