LORD CoolTherm™ EP-636 epoxy encapsulant is a two-component system specifically designed for high temperature applications. CoolTherm EP-636 encapsulant is recommended for encapsulation of electric motor stator assemblies used on downhole oil pumps. CoolTherm EP-636 hardener may crystallize during shipment or storage. If crystals appear, gently warm hardener at 50-65°C to melt crystals before mixing with resin. Features: maintains electrical insulation stability at extremely high temperatures. provides protection of electrical devices exposed to harsh environmental conditions. exhibits very low weight loss over extended periods at elevated temperatures. All information provided by Lord. |