MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ 4031 PBT (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric motors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Density 1.54 g/ccISO 1183
Filler Content 30 %ASTM D229
Water Absorption 0.26 %23°C/sat; ISO 62
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Viscosity 150 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.010 cm/cmSABIC method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 30 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 40 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 50 g/10 min
@Load 5.00 kg,
Temperature 266 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ISO 2039-2
Ball Indentation Hardness 125 MPaISO 2039-1
Tensile Strength at Break 135 MPa5 mm/min; ISO 527
 140 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 135 MPa5 mm/min; ISO 527
 140 MPa5 mm/min; ASTM D638
Elongation at Break 2.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Elongation at Yield 2.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Tensile Modulus 10000 MPa5 mm/min; ASTM D638
 10000 MPa1mm/min; ISO 527
Flexural Strength 190 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 200 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 190 MPa1.3 mm/min, 50 mm span; ASTM D790
 210 MPa2 mm/min; ISO 178
Flexural Modulus 7900 MPa1.3 mm/min, 50 mm span; ASTM D790
 8300 MPa2 mm/min; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; ISO 178
Izod Impact, Notched 100 J/mASTM D256
 100 J/m
@Temperature -30.0 °C
ASTM D256
 100 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Unnotched 880 J/mASTM D4812
 880 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²80*10*4; ISO 180/1U
 55.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 50.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 65.0 kJ/m²ISO 179/2C
 55.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 12.0 kJ/m²ISO 179/2C
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.1
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 24.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 24.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 0.800 mm
in oil; ASTM D149
Dissipation Factor 0.0016
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 VIEC 60112
 >= 600 VUL 746A
Hot Wire Ignition, HWI 60 - 120 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 21.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 120 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 173 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 220 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 220 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 210 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 215 °CRate B/50; ISO 306
 215 °CRate B/50; ASTM D1525
 215 °CRate B/120; ISO 306
 220 °CRate A/50; ASTM D1525
 220 °CRate A/50; ISO 306
UL RTI, Electrical 140 °CUL 746B
UL RTI, Mechanical with Impact 140 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 HB
@Thickness 0.840 mm
UL 94
 HB
@Thickness 6.00 mm
UL 94
Glow Wire Test 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10250 / 243717

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.