MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® Centrex® 825/LXS ASA/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: Co-extruded ASA/High Impact ABS Sheet (High Gloss)

ALLEN® Centrex® 825/LXS is high impact ABS capped with Centrex® ASA for UV protection and high gloss finish.

ALLEN® Centrex® 825/LXS is Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94) and Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302)

Suggested Applications:

  • Vehicle Exteriors
  • Marine Parts
  • Radomes
  • Agriculture Equipment Exteriors
  • Construction Equipment Exteriors
  • Lift Boom Exteriors

Features:

  • Custom color matching
  • Excellent UV properties
  • Edge trim easily used into future orders
  • High gloss finish
  • Good chemical resistance
  • Color and gloss retention

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 - 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 34.4 MPaASTM D638
Flexural Strength 55.9 MPaASTM D790
Flexural Modulus 1999.4 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Temperature -17.8 °C
ASTM D256
 320 J/m
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Optical PropertiesOriginal ValueComments
Gloss >= 85 %60° Angle; ASTM D523
 
Descriptive Properties
Motor Vehicle Safety StandardPassesFMVSS 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HS6500 High Impact ABS Resin
SEKISUI SPI ALLEN® 3800/LXS ABS
SEKISUI SPI ALLEN® 3800/499 ABS
Ravago Manufacturing Americas Hylac® EX28 ABS
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin

PSEKIS020 / 185845

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.