MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary Evoprene™ GF 6250 Automotive Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitable for automotive interior applications.
Processing: can be injection molded or extruded on standard thermoplastics equipment
Applications: trinket mats, handbrake grips and gear knobs, pillar trim skins, vent wheels, seat belt scabbards & other seating components, armrest skins, bump stops
Formulated to meet the requirements of automotive Gravimetric Fogging standard DIN 75201B

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 47ISO 868, 15 sec
Tensile Strength 6.20 MPa500 mm/min, measured parallel to flow; ISO 37
Elongation at Break 550 %500 mm/min, measured parallel to flow; ISO 37
100% Modulus 0.00280 GPa
@Strain 100 %
500 mm/min, measured parallel to flow; ISO 37
Tear Strength 17.0 kN/mParallel to flow; ISO 34-B
 33.0 kN/mPerpendicular to flow; ISO 34-B
Compression Set 20 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 33 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
Tensile Set 45 %
@Temperature 70.0 °C,
Time 79200 sec
VDA 675 217B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
@Time 10800 sec
no distortion
Brittleness Temperature -60.0 °CASTM D 746
Flame Spread 42 mm/minburn rate
 
Descriptive Properties
Odor Rating2SAE J1351 / FLTM BO131-01
Ozone Resistance0100 pphm / 200 hrs / 20% strain

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® TPU GF20 20% Glass Filled
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
Avient Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
AlphaGary Evoprene™ G 996 SEBS Thermoplastic Elastomer

PGARY9636 / 140429

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.