MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gougeon Brothers PRO-SET® ACE-166/ACE-265 Absolute Clear Coating Epoxy- Slow
Categories: Polymer; Thermoset; Epoxy

Material Notes: Formulated for extremely clear coatings and laminations with carbon and other reinforcement fibers. Commonly used for clear coatings on wood, surfboard laminations and other board sport products in a production setting. Provides colorless clarity and UV stability. For ultimate long-term UV stability, use with a UV stable top coat.
Slow cure speed for fill coating, laminating and potting. Slow hardener provides a tack-free cure time of approximately 4 hours at 72°F (22°C).
Easy processing for hand wet out of lightweight reinforcement fabrics or fibers. Provides extremely smooth surface when cured1. Excellent sandability. Reaches full physical properties at room temperature cure.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccHardener
 1.15 g/ccCured
 1.17 g/ccResin
Viscosity 661 cP
@Temperature 29.0 °C
Mixed; ASTM D2196
 878 cP
@Temperature 25.0 °C
Mixed; ASTM D2196
 1054 cP
@Temperature 22.0 °C
Mixed; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D2240
Tensile Strength 8840 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D638
Elongation at Break 2.6 %
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D638
Tensile Modulus 507000 psiASTM D638
Flexural Strength 13900 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D790
Flexural Modulus 478000 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D790
Compressive Yield Strength 13400 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D695
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 122 °F
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D648
Glass Transition Temp, Tg 122 °F
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
DSC Onset– 1st Heat; ASTM E1356
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 hour
@Temperature 29.4 °C
tack-free time
 3.75 hour
@Temperature 25.0 °C
tack-free time
 4.00 hour
@Temperature 22.2 °C
tack-free time
Pot Life 16.0 - 20.0 min
@Load 0.150 kg,
Temperature 29.0 °C
ASTM D2471
 16.0 - 20.0 min
@Load 0.500 kg,
Temperature 29.0 °C
ASTM D2471
 21.0 - 27.0 min
@Load 0.500 kg,
Temperature 25.0 °C
ASTM D2471
 24.0 - 30.0 min
@Load 0.150 kg,
Temperature 25.0 °C
ASTM D2471
 26.0 - 32.0 min
@Load 0.500 kg,
Temperature 22.0 °C
ASTM D2471
 26.0 - 33.0 min
@Load 0.150 kg,
Temperature 22.0 °C
ASTM D2471
Shelf Life 24.0 Monthhardener
 36.0 Monthresin
 
Descriptive Properties
Mix ratio1.96:1—2.26:1Volume Range, Resin: Hardener
 100:41.9Weight, Resin: Hardener
 100:42.9—100:37.0Weight Range, Resin: Hardener
 100:50.0Volume, Resin: Hardener
 100:51.1—100:44.2Volume Range, Resin: Hardener
 2.00:1Volume, Resin: Hardener
 2.33:1—2.70:1Weight Range, Resin: Hardener
 2.39:1Weight, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGP949 / 290792

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.