MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Insulating Firebricks JM 23 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes:

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.480 g/cc
@Temperature 23.0 °C
at 50% RH; ASTM C-134-84
Deformation 0.10 %
@Temperature 1100 °C,
Time 5400 sec
Hot Load Strength, 0.034 Mpa; ASTM C-16
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00100 GPa
@Temperature 23.0 °C
at 50% RH; ASTM C-93-84
Compressive Strength 1.20 MPaCold Crushing Strength, 50% RH; ASTM C-93-84
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.120 W/m-K
@Temperature 400 °C
 0.140 W/m-K
@Temperature 600 °C
 0.170 W/m-K
@Temperature 800 °C
 0.190 W/m-K
@Temperature 1000 °C
Shrinkage 0.20 %
@Time 86400 sec
after soaking; ASTM C-210
 
Component Elements PropertiesOriginal ValueComments
Al2O3 37 %
CaO 15.2 %
Fe2O3 0.70 %
MgO 0.30 %
SiO2 44.4 %
TiO2 1.2 %
 
Descriptive Properties
Classification Temperature (°C)1260
Reversible Linear Thermal Expansion Max (%)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Nextel™ 610 Composite Ceramic Fiber
Thermal Ceramics Min-K Type LW Insulating Tape
Thermal Ceramics Min-K Type HT Insulating Tape
Thermal Ceramics Min-K Standard Insulating Tape
Thermal Ceramics Min-K Moldable

CMORF6013 / 202797

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.