CS Glass Sands are functional fine aggregate materials made with uniform grain size distributions from 100% recycled glass: CS Glass from bottle glass and a greenish tan in color. CS Glass Sands are free of crystalline silica and provide a clean recycled sand for concrete, polymer concrete, mortars, and other similar systems. The products are very low in lead (Pb) content and free of label remnants and other post consumer debris.Information provided by Vitro Minerals. |