MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess Addolink® 0312 Crosslinking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Preparation: Prior to processing, Addolink 0312 is being molten in a circulating air oven (guideline: to melt 8 kg will take approx. 5 hours) and thoroughly homogenized by stirring or shaking or the extremely low water content of the product will concentrate locally. Addolink 0312 has to be kept liquid at 70 - 80 °C, but only in such quantities which may be processed within 8 hours. Once in a liquid state, the crosslinker has to be protected from moisture.

Function: Crosslinker for polyurethane hot-curing cast elastomers.

Application: Addolink 0312 is a slowly reacting crosslinker and is used in liquid form for the production of polyurethane hot-curing cast elastomers based polyesterpolyols / NDI, polyesterpolyols / MDI and for MDI-prepolymers. By use of Addolink 0312, cast time is prolonged up to 30 minutes; demolding is possible within one hour.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/cc
Water Absorption <= 0.10 %
Viscosity 70 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point 60.0 °C
Flash Point 176 °CCleveland open cup; DIN ISO 2592
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceyellowish to brown solid
Hydroxyl value760 mg KOH/g
Specifications98 percentActive ingredient

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8202 / 208595

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.