MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arya Sasol HFI 5110 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HFI5110 is a high molecular weight, high-density polyethylene with broad molecular weight distribution specially developed for producing thin films with excellent strength and rigidity. This product is suitable for manufacture of high strength grocery sacks, shopping bags and high quality thin films for uni/multi-wall packaging. Films produced with this grade can be readily treated and printed to give high quality graphics. HFI5110 has been manufactured under Basell license.

Application: Blown film extrusion, uni/multi wall packaging, high quality thin films, shopping bags, high strength grocery sacks

Forms: Pellets

Attribute: High tear resistance, high melt stability, high quality graphic printing

Additives: Antioxidant: Yes; Zinc Stearate: Yes; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccISO 1183
Thickness 15.0 - 50.0 microns
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaISO 527-1, -3
Film Elongation at Break, MD 580 %ISO 527-1,3
Film Elongation at Break, TD 620 %ISO 527-1,3
Elongation at Yield 10 %ISO 527-1, -3
Modulus of Elasticity 1.05 GPaISO 527-1,3
Elmendorf Tear Strength MD 25.5 gISO 6383-2
Elmendorf Tear Strength TD 81.5 gISO 6383-2
Film Tensile Strength at Break, MD 55.0 MPaISO 527-1,3
Film Tensile Strength at Break, TD 55.0 MPaISO 527-1,3
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °CISO 3146
Vicat Softening Point 127 °C
@Load 1.02 kg
Method A; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 235 °CExtruder temperature profile
Blow-up Ratio (BUR) 2.0 - 5.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARYA009 / 250463

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.