MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kingfa PA6-T25 25% Mineral Filled PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes:
    Features:
  • Low tendency to wrap

    Applications:
  • Injection molding
  • Sport appliance
  • Automobile parts
  • Power tools

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/cc
@Temperature 23.0 °C
ASTM D792
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength at Break 80.0 MPa10mm/min; ASTM D638
Elongation at Break >= 10 %50mm/min; ASTM D638
Flexural Strength 120 MPa2mm/min; ASTM D790
Flexural Modulus 4700 MPa2mm/min; ASTM D790
Izod Impact, Notched 65.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
Rear Barrel Temperature 225 - 245 °CStart Point: 230°C
Middle Barrel Temperature 250 - 270 °CStart Point: 255°C
Front Barrel Temperature 260 - 280 °CStart Point: 265°C
Melt Temperature 255 - 285 °CStart Point: 265°C
Mold Temperature 50.0 - 70.0 °CStart Point: 60°C
Drying Temperature 90.0 - 110 °C
@Time 14400 - 21600 sec
Pre-dry
 
Descriptive Properties
Injection SpeedModerate to High
Mineral Content (%)25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa PA66-RG001 Flame Retardant PA66
Kingfa LONOY 2100 LT PC/PET Alloy
Kingfa LONOY 1300 PC/PBT Alloy
Kingfa PA66-RG201 Flame Retardant, 20% Glass Fiber Reinforced PA66
Kingfa PBT-T15 15% Mineral Filled PBT

PKINGF028 / 104287

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.