MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX973 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 973 resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less electrostatic and powder coat painting. NORYL GTX973 resin exhibits high impact resistance and strength and is an excellent candidate for automotive painted applications such as body panels, fenders, and tank flaps.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Low Warpage,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Density 1.10 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 1.20 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 4.2 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa50 mm/min; ASTM D638
 55.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
Elongation at Break 30 %50 mm/min; ISO 527
 55 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2200 MPa50 mm/min; ASTM D638
 2300 MPa1 mm/min; ISO 527
Flexural Strength 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 90.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
 2300 MPa2 mm/min; ISO 178
Izod Impact Notched 130 JASTM D256
 80.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 - 10000 ohm-cmSABIC method
Comparative Tracking Index 100 - 175 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 195 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 195 °CRate B/50; ISO 306
 200 °CRate B/50; ASTM D1525
 200 °CRate B/120; ISO 306
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 675 °C
@Thickness 2.00 mm
IEC 60695-2-13
 675 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 675 °C
@Thickness 2.00 mm
IEC 60695-2-12
 675 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 280 - 300 °C
Zone 3 290 - 320 °C
Melt Temperature 290 - 320 °CInjection Molding
Mold Temperature 100 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82189 / 290136

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.