MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker Geniosil® XL 65 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C6H15NO4Si

CAS No.: 23432-65-7

Properties: GENIOSIL® XL 65 is characterized by its high reactivity toward moisture, a direct consequence of the structural proximity of the nitrogen atom to the silicon atom (alpha-effect).On account of its highly reactive nature, GENIOSIL® XL 65 is of substantial importance in systems that cure very rapidly at room temperature on exposure to (atmospheric) moisture. This applies particularly to formulations in which alphaorganofunctional terminal groups function as crosslinkers. The addition of GENIOSIL® XL 65 greatly improves the storage stability. GENIOSIL® XL 65 is especially suitable for producing highly flexible products with a low modulus of elasticity. This is because the dialkoxysilyl group functions as a chain extender during curing of the prepolymer, producing a lower degree of crosslinking.

Special features: GENIOSIL® XL 65 is an alkoxysilane with an O-methyl carbamate organofunctional group. It´s a clear, colorless to light yellowish liquid with a characteristically aromatic odor. The silane hydrolyzes in the presence of moisture (methanol is released) to form silanols, which can then react with themselves to produce siloxanes. The close proximity of the nitrogen atom to the silicon atom results in a greatly accelerated hydrolysis reaction (alphaeffect). GENIOSIL® XL 65 is a highly reactive molecule capable of scavenging water in formulations.

Application: GENIOSIL® XL 65 is used as a water scavenger in the production of moisture-curing adhesive and sealant formulations. It is important particularly in systems using highly reactive silane-modified polymers basedon alpha-organofunctional silanes. As a bifunctional silane, GENIOSIL® XL 65 functions additionally as a chain extender and is thus ideally suited for highly flexible products.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.1025 g/ccEU-FL.A.3
Kinematic Viscosity 3.25 cSt
 
Thermal PropertiesOriginal ValueComments
Boiling Point 211.1 °CEU-GL.A.2
Flash Point 112 °CISO 3679
Ignition Temperature 250 °CEU-GL.A.15
 
Descriptive Properties
Purity>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9337 / 204866

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.