MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECARAN ABS natural Acrylonitrile-butadiene-styrene copolymer
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes:
  • electrically insulating
  • high stiffness
  • good chemical resistance
  • low density
  • good damping
  • high toughness
  • low moisture absorption
Target Industries:
  • food processing
  • home appliances
  • automotive industry
  • fixture construction
  • food engineering
  • electronics
  • medical technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Moisture Absorption 0.700 %saturation; ASTM D570
 0.130 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Hardness, Shore D 78ASTM D2240
Tensile Strength at Break 4000 psiASTM D638
Tensile Strength, Yield 5800 psiASTM D638
Elongation at Break 30 %ASTM D638
Elongation at Yield 2.0 %ASTM D638
Modulus of Elasticity 400 ksiASTM D638
Flexural Strength 8900 psiASTM D790
Flexural Modulus 310000 psiASTM D790
Compressive Yield Strength 7100 psi
@Strain 10 %
ASTM D695
Compressive Strength 3200 psi
@Strain 1 %
ASTM D695
Compressive Modulus 375000 psiASTM D695
Izod Impact, Notched 5.30 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.35
@Pressure 0.276 MPa
50 fpm; ASTM D3702
Coefficient of Friction, Static 0.19 - 0.21ASTM D3702
K (wear) Factor 3500 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+14 ohmASTM D257
Dielectric Constant 3.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.7 kV/mmASTM D149
Dissipation Factor 0.020
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 56.0 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM D696
Maximum Service Temperature, Air 160 °FLong Term
 210 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 200 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 177 °FASTM D648
Vicat Softening Point 224 °F
Glass Transition Temp, Tg 220 °FASTM D3418
Flammability, UL94 HB
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8199 / 319127

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.