MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® MDF35 Nylon 6, Dry, 35% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Notes: MDF35 is a 35% glass fiber reinforced nylon 6 that offers superior mechanical performance coupled with good surface finish and molding release characteristics.

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 35% Filler by Weight

Features: Good Mold Release; Good Surface Finish

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Moisture Absorption at Equilibrium 1.9 %50% RH; ISO 62
Linear Mold Shrinkage 0.0070 - 0.012 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 26100 psiISO 527-2
Elongation at Break 4.0 %ISO 527-2
Tensile Modulus 1.45e+6 psiISO 527-2
Flexural Strength 37700 psiISO 178
Flexural Modulus 1.33e+6 psiISO 178
Izod Impact, Notched (ISO) 6.70 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 26.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 8.10 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.8IEC 60250
Dielectric Strength 280 V/mil
@Thickness 3.00 mm
IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 392 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) >= 392 °FUnannealed; ISO 72-2/A
Flammability, UL94 HB
@Thickness 0.762 mm
Black only
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 482 - 536 °F
Middle Barrel Temperature 482 - 536 °F
Front Barrel Temperature 482 - 536 °F
Melt Temperature 482 - 536 °F
Mold Temperature 158 - 194 °F
Drying Temperature 176 °F
Dry Time 20.0 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0591 / 237082

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.