MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Beetle® A82 Nylon 66, Non-Halogenated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Notes: A82 is a UL recognized. V-0 rated halogen and phosphorus-free flame retarded, heat stabilized, unreinforced injection molding grade of nylon 66.

Features: Flame Retardant; Heat Stabilized; Halogen Free; Low (to no) phosphorus content

Processing Method: Injection Molding

Forms: Pellets

Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: Fast

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 0.569 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 518 - 554 °F
Middle Barrel Temperature 518 - 554 °F
Front Barrel Temperature 518 - 554 °F
Melt Temperature <= 572 °FProcessing Temperature
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F
Dry Time 2 hour
Screw Speed 50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6
BASF Ultramid® 8202C HS PA6 (Conditioned)
BASF Ultramid® 1000-2 NF2001 PA66 (Conditioned)

PTEKNO441 / 128618

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.