Lupolen 3426 J is an additivated, low density polyethylene. It contains slip and anti-blocking agent. It is characterized by a good processability and high stiffness. LyondellBasell customers report that Lupolen 3426 J is used in hygiene film and that films made from Lupolen 3426 J exhibit a glossy surface finish. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Hygiene Film, Lamination FilmInformation provided by LyondellBasell. |