MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccISO 1183
Bulk Density 0.700 g/ccISO 60
Linear Mold Shrinkage, Flow 0.0010 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0030 cm/cm60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0020 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0070 cm/cm60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaISO 527-1, -2; 5 mm/min
Elongation at Break 2.9 %ISO 527-1, -2; 5 mm/min
Tensile Modulus 7000 MPaISO 527-1, -2; 1 mm/min
Flexural Strength 170 MPa
@Strain 3.2 %
2 mm/min; ISO 178-A
Flexural Modulus 7000 MPa2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1, -3
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °C
 270 °Cfor test specimens; ISO 294
Mold Temperature 80.0 - 100 °C
 90.0 °Cfor test specimens; ISO 294
Drying Temperature 120 °C
Dry Time 4 - 8 hour
Moisture Content 0.00 - 0.020 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 7792-1-PBT+ASA, GHMR, 07-070, GF20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber
Envalior Pocan® A 3121 000000 PBT+ASA, 20% Glass Fiber Reinforced
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT + ASA
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
Envalior Pocan® AF 4120 000000 PBT+ASA, 20% Glass Fiber Reinforced

PLANX0671 / 133634

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.