MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ertalon® 6 SA PA 6, extruded (ISO Data)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulating properties and a good chemical resistance make Ertalon 6 SA a “general purpose” grade for mechanical construction and maintenance.

  • High mechanical strength, stiffness, hardness and toughness
  • Good fatigue resistance
  • High mechanical damping ability
  • Good sliding properties
  • Excellent wear resistance
  • Good electrical insulating properties
  • Good resistance to high energy radiation (gamma- and X-rays)
  • Good machinability

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183-1
Moisture Absorption at Equilibrium 2.6 %50% RH
Water Absorption at Saturation 9.0 %
Outgassing - Total Mass Loss 1.3 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ISO 2039-2
Hardness, Shore D 79
Ball Indentation Hardness 150 MPaISO 2039-1
Tensile Strength, Yield 80.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
Tensile Modulus 3300 MPaISO 527-1/-2
Flexural Strength 116 MPa
Flexural Modulus 3080 MPa
Compressive Strength 31.0 MPa
@Strain 1 %
ISO 604
 59.0 MPa
@Strain 2 %
ISO 604
 87.0 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 19 µm/km
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 5.50 kJ/m²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.40 - 0.60
Limiting Pressure Velocity 0.0700 MPa-m/secat 1 m/s unlubricated
 0.120 MPa-m/secat 0.1 m/s unlubricated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.0e+14 ohm-cmIEC 60093
Surface Resistivity per Square >= 1.0e+13 ohmIEC 60093
Dielectric Constant 3.9
@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
Dissipation Factor 0.019
@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 105 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.280 W/m-K
Melting Point 220 °CDSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 70.0 °CContinuous; 20,000 h
 85.0 °CContinuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75-1/-2
Flammability, UL94 HB
Oxygen Index 25 %ISO 4589-1/-2
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
European Food 1935/2004 Yes
FDA Yesonly natural
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA PA66 AE Polyamide 66, extruded
Overview of materials for Nylon 6, Cast
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber
Mitsubishi Chemical Advanced Materials Nylatron™ GF30 / Ertalon™ 66 GF30 PA66 30% glass filled, extruded
Overview of materials for Nylon 6, Extruded

P1SMU842 / 130661

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.