MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR Resin ENH4565 Polybutylene Terephthalate (PBT) (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: VALOX ENH4565 is a 33% glass reinforced, non-chlorinated/brominated flame retardant Polybutylene Terephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.75mm flame rating. This is a good candidate for a variety of applications needing a sustainable FRPBT solution.

Features: Chemical Resistance,Flame Retardant,Non-Chlorinated,Non-Brominated,ECO Compliant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D792
Density 1.61 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %ISO 62-1
Viscosity 18 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
 20 cP
@Load 5.00 kg,
Temperature 265 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cmSABIC method
 0.0010 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cmSABIC method
 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 137 MPa5 mm/min; ASTM D638
 140 MPa5 mm/min; ISO 527
Tensile Strength, Yield 137 MPa5 mm/min; ASTM D638
 140 MPa5 mm/min; ISO 527
Elongation at Break 2.4 %5 mm/min; ASTM D638
 2.4 %5 mm/min; ISO 527
Elongation at Yield 2.4 %5 mm/min; ASTM D638
 2.4 %5 mm/min; ISO 527
Tensile Modulus 11500 MPa1 mm/min; ISO 527
 11600 MPa5 mm/min; ASTM D638
Flexural Strength 180 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 185 MPayield, 2 mm/min; ISO 178
Flexural Modulus 9400 MPa1.3 mm/min, 50 mm span; ASTM D790
 9400 MPa2 mm/min; ISO 178
Izod Impact Notched 80.0 JASTM D256
 60.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 800 J/mASTM D4812
 600 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²80*10*4; ISO 180/1A
 14.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact Unnotched 60.0 kJ/m²ISO 179/2C
 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 12.0 kJ/m²ISO 179/2C
 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 9.00 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 19.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 20.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 98.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 205 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 255 °C
Zone 2 235 - 250 °C
Zone 3 240 - 260 °C
Melt Temperature 245 - 260 °CInjection Molding
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82783 / 290730

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.