Fast, aggressive tack for bonding many lightweight materials. Choice of round or fan pattern nozzle. Spray width 1"-3" variable. Bonding range surfaces: one side 15 minutes, both sides 30 minutes. Peel strength is 15 PIW; ITSD T.M. C-449. Coverage is 220 square feet per 24 ounce container. Information provided by 3M Adhesives Division. |