MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chesterton MRS SD4i Metal Rebuilding System
Categories: Ceramic

Material Notes: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shrinking, 100% solids. MRS SD4i formulated for the resurfacing of metal components subjected to extreme corrosive or severe fluid flow conditions. MRS SD4i is a low viscosity composite that is designed to be spray applied but may also be applied by roller or brush. This product is designed as a two coat system to provide extended life for plant equipment. Cured MRS SD4i provides a high gloss ceramic surface with resistance to erosion-corrosion and permeation.

Benefits:

  • High loading of ceramic reinforcements extends equipment services life against wear.
  • Exceptional resistance to blistering and chemical attack during long term immersion conditions
  • High gloss finish reduces drag, improves pump efficiency on warn components
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance against underfilm corrosion
  • Convenient 2 -1 volumetric mix ratio and verification of mis by color change.

Suggested Uses:

  • Chemical Storage Tanks
  • Exhaust Gas Ductwork
  • Heat Exchangers
  • Tank Linings
  • Chimneys and Stacks
  • Fans and Housings
  • Chemical Piping

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D2240
Tensile Strength at Break 3800 psiASTM D638
Elongation at Break 2.8 %ASTM D638
Flexural Strength 9100 psiASTM D790
Flexural Modulus 880000 psiASTM D790
Compressive Strength 13100 psiASTM D695
Adhesive Bond Strength >= 2000 psiTensile; ASTM D4541
Taber Abrasion, mg/1000 Cycles 26
@Load 1.00 kg
H-18, loss; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 65.0 °CWet
 120 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 hour
@Temperature 32.0 °C
Light Load
 10.0 hour
@Temperature 25.0 °C
Light Load
 10.0 hour
@Temperature 32.0 °C
Overcoat End
 14.0 hour
@Temperature 32.0 °C
Full Load
 18.0 hour
@Temperature 16.0 °C
Light Load
 20.0 hour
@Temperature 25.0 °C
Overcoat End
 24.0 hour
@Temperature 10.0 °C
Light Load
 24.0 hour
@Temperature 25.0 °C
Full Load
 24.0 hour
@Temperature 32.0 °C
Full Chemical
 30.0 hour
@Temperature 16.0 °C
Overcoat End
 40.0 hour
@Temperature 10.0 °C
Overcoat End
 48.0 hour
@Temperature 16.0 °C
Full Load
 48.0 hour
@Temperature 25.0 °C
Full Chemical
 60.0 hour
@Temperature 10.0 °C
Full Load
 96.0 hour
@Temperature 16.0 °C
Full Chemical
 120 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 1.00 hour
@Temperature 32.0 °C
 4.00 hour
@Temperature 16.0 °C
 6.00 hour
@Temperature 10.0 °C
 30.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorBlue
 Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
Crystex Composites Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
CoorsTek PlasmaPure-UC™ 99.9% Alumina
CoorsTek PlasmaPure™ AD-998 Alumina (nom. 99.8% Al2O3)

PPTCHS126 / 138238

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.