MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ixom ASTALOY™ PC/ABS TWG
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ASTALOY™ PC/ABS TWG is a high weldline impact strength alloy of ABS and Polycarbonate and is designed for injection molding applications with multiple weldlines and requiring a balance of impact toughness, heat resistance, product rigidity, mouldability and easy painting. Typical applications in the automotive area are interior instrument panel fascia panels, console capping moldings and glove box assemblies, together with exterior painted components such as wheel trims, front grilles, rear appliques and other trim panels.

Information provided by Ixom Operations PTY LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Water Absorption 0.25 %
@Time 86400 sec
ASTM D570
Melt Flow 4.6 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 10 g/10 min
@Load 3.80 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength 51.0 MPa12.7 mm x 3.2 mm @ 5.0 mm/min; ASTM D638
Elongation at Break 70 %12.7 mm x 3.2 mm @ 5.0 mm/min; ASTM D638
Flexural Strength 90.0 MPa12.7 mm x 3.2 mm @ 1.3 mm/min; ASTM D790
Flexural Modulus 2630 MPa12.7 mm x 3.2 mm @ 1.3 mm/min; ASTM D790
Izod Impact, Notched 510 J/m12.7 mm x 3.2 mm; ASTM D256
Falling Dart Impact 60.0 J3.2 mm plaque; ASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 102 °C12.7 mm x 3.2 mm; ASTM D648
Vicat Softening Point 135 °C
@Load 1.00 kg
ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
Shrinkage 0.60 %3.0 mm plaque; ASTM D955
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 235 - 255 °C
Middle Barrel Temperature 245 - 265 °C
Front Barrel Temperature 255 - 275 °C
Melt Temperature 250 - 280 °C
Mold Temperature 50.0 - 90.0 °C
Drying Temperature 95.0 - 100 °CTemperature of pellet bed
Dry Time 3.00 - 5.00 hourat desired pellet bed
Injection Pressure 60.0 - 140 MPa
Back Pressure 0.100 - 0.500 MPa
Screw Speed 40 - 60 rpm
 
Descriptive Properties
Clamp pressure4 - 8 kN/cm²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PIXOM016 / 283097

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.