MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured product have some flexibility so it resists cracking and chipping and cracking with an impact force. This foam may be used in production of small to medium light parts with some structural integrity.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °FPrepolymer Temperature
 70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 100 - 110 °F
Cure Time 0.670 - 1.00 hour
@Temperature 43.3 °C
De-mold Time
 24.0 - 48.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 0.500 - 0.670 min
 
Descriptive Properties
Curing AgentPAC-004
Mixing Time10-15by hand
PrepolymerMPN-023
Weight Ratio1:0.212Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORTH878 / 162594

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.