MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polikim KESTAMID® HS Polyamide 6, Heat Resistant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with a longer duration compared to other extrusion and cast polyamide types. Its continuous operating temperature increases by 15-30°C compared to Kestamid® and reaches the 125-140°C interval. Thanks to its short term operating temperature that reaches 185-200°C interval, it is used safely in many applications that require heat resistance.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Water Absorption at Saturation 6.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84ISO 868
Tensile Strength, Ultimate 800 kg(f)/cm²ISO 527
Elongation at Break >= 20 %ISO 527
Tensile Modulus 4000 MPaISO 527
Compressive Strength 950 kg(f)/cm²ISO 604
Compressive Modulus 2700 MPaISO 604
Izod Impact, Notched (ISO) 5.60 kJ/m²ISO 180
Charpy Impact Unnotched NBISO 179
Coefficient of Friction 0.39
K Factor (Wear Factor) 0.44[mg/km]
K (wear) Factor 500 x 10-8 mm³/N-M
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmISO 60093
Surface Resistance >= 1.00e+13 ohmISO 60093
Dielectric Constant 3.7ISO 60250
Dielectric Strength 25.0 kV/mmISO 50243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CISO 11359
Melting Point 220 °C
Maximum Service Temperature, Air 125 °Ccontinuous
 185 °Cshort term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polikim KESTAMID® PA6G Polyamide 6
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
A. Schulman BMC 695 Vinyl Ester Molding Compound
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
Bakelite® Keripol® RW 1411 Polyester Molding Compound, Low Shrinkage, Resistant to High Temperatures

PPOLIK014 / 99824

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.