MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 9009 Double Coated Tapes with Adhesive 300
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides relatively high initial adhesion and good shear holding power to a variety of surfaces. The carrier also provides easier handling during slitting and die cutting.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.500 milCarrier
 0.800 milFaceside Adhesive
 0.800 milBackside Adhesive
 2.10 milTape
 3.00 milLiner Caliper
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 3.375 plito stainless steel, 90°, 15 min RT; ASTM D3330
 3.6875 plito ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 3.8125 plito stainless steel, 90°, 72 hr RT; ASTM D3330
 3.8125 plito Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 4.75 plito stainless steel, 90°, 72 hr at 70°C; ASTM D3330
 5.125 plito stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °CLong term
 121 °CShort term
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33268 / 168015

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.