MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
TBA ECP 16E Stainless Steel Fiber Masterbatch
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Typical Physical Properties in ABS

ECP 16E is a stainless steel fiber masterbatch within a Nylon 6/12 binder, 25% by weight. It can be used with Nylon 6, 6/6, 6/10, 6/12, PBT, PET. Other binders are available - ECP 12E using Emulsion based ethylene acrylic acid sincionomer binder, 25% by weight for use with Styremic Thermoplastics, PS, SAN, ABS, also PPO and PPE Alloys, Polypropylene/Polyolefines. ECP 20E with a polycarbonate binder 40% by weight, for use with polycarbonate, polysulphone, PES, PET, PEJ, PBT. The masterbatch is added at very low levels ensuring minimal effect on color, moldability and other base polymer properties by 1% by volume. The use of this system allows shielded articles to be produced in one process without additional equipment, labor or secondary processing and provides cost effective solution to EMI shielding problems.

Features:

  • No secondary process
  • Used in any plastic molding application
  • Can be colored (but not suitable for bright colors such as yellow, white etc)
  • Provides shielding of 50dB attenuation
Benefits:
  • Cost effective
  • Non-abrasive
  • Minimal effect on color
  • Eliminates secondary shielding process

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 32.3 MPa
Elongation at Break 3.5 %
Tensile Modulus 2360 MPa
Flexural Strength 58.0 MPa
Flexural Modulus 2190 MPa
Izod Impact, Notched 55.1 J/m
Charpy Impact Unnotched 15.9 kJ/m²
Charpy Impact, Notched 7.10 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTBA004 / 281482

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.