MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRES™ ML0111 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES ML0111 is based on Polycarbonate (PC) siloxane copolymer resin with high flow, high impact resistance performance and colorable. This is an injection molding (IM) grade and especially suitable for IMT/IML process.

Features: Colorable,High Impact Resistance,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Density 1.18 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.430 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm24hrs; ASTM D955
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 92ASTM D785
Tensile Strength at Break 47.0 MPa50 mm/min; ISO 527
 54.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa50 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
Elongation at Break 46 %50 mm/min; ISO 527
 76 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ASTM D638
 4.5 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1 mm/min; ISO 527
 2380 MPa50 mm/min; ASTM D638
Flexural Strength 93.0 MPa2 mm/min; ISO 178
 97.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2400 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 753 JASTM D256
 124 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 51.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
Charpy Impact Unnotched NBISO 179/2C
Charpy Impact, Notched 55.0 kJ/m²ISO 179/2C
 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 62.0 JASTM D3763
 62.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.8
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor 0.0060
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 110 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 110 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 100 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 117 °CRate B/50; ISO 306
 119 °CRate B/120; ISO 306
 125 °CRate B/50; ASTM D1525
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °C
Zone 2 275 - 295 °C
Zone 3 280 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 100 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80596 / 288543

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.