MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond A134 Anaerobic Retainer
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Permabond® A134 is a high-strength anaerobic product designed for the permanent locking and sealing of metal parts. Its 'non-drip' formulation makes it suitable for use on larger fittings, coarse threads or for the renovation of assemblies where wide tolerances are expected due to damage or wear. A134 can extend the life of components by reducing the effects of corrosion in aggressive environments.

Features & Benefits

  • Easy to apply
  • Thixotropic
  • Room temperature cure
  • Very high strength
  • Excellent chemical resistance
  • WRAS listed for contact with wholesome (potable) water

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccUncured
Viscosity 8000 cP
@Temperature 25.0 °C
at 20 rpm vibration
 70000 cP
@Temperature 25.0 °C
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 21.0 MPasteel collar and pin shear; ISO 10123
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 11.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
Thermal Conductivity 0.190 W/m-K
 
Processing PropertiesOriginal ValueComments
Cure Time 0.0830 hour
@Temperature 23.0 °C
Brass, handling strength
 0.250 hour
@Temperature 23.0 °C
Zinc, handling strength
 0.250 hour
@Temperature 23.0 °C
M10 steel, handling strength
 0.500 hour
@Temperature 23.0 °C
Brass, working strength
 1.00 hour
@Temperature 23.0 °C
M10 steel, working strength
 6.00 hour
@Temperature 23.0 °C
Zinc, working strength
 6.00 hour
@Temperature 23.0 °C
Stainless steel, handling strength
 24.0 hour
@Temperature 23.0 °C
M10 steel, full strength
 
Descriptive Properties
AppearanceGreenUncured
Maximum Gap Fill (mm)0.5
Maximum Thread SizeM80
Strength Retention50% at 150°CRelative to 0°C
 80% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C
Torque Strength (N m)25M10 Zn plated, break
 30M10 steel, break
 45M10 Zn plated, prevail
 50M10 steel, prevail
UV FluorescenceYesUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERMA808 / 162733

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.