MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Information provided by Bayer Corporation, Plastics Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Linear Mold Shrinkage 0.0080 cm/cmASTM D955
Spiral Flow 51.0 cm
@Thickness 2.50 mm
at 254°C melt temp.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 55.0 MPaASTM D638
Elongation at Break 82 %ASTM D638
Tensile Modulus 2.60 GPaASTM D638
Flexural Yield Strength 92.0 MPaASTM D790
Flexural Modulus 2.34 GPaASTM D790
Izod Impact, Notched 4.20 J/cm
@Temperature -40.0 °C
ASTM D256
 7.50 J/cm
@Thickness 3.17 mm
ASTM D256
Instrumented Impact Total Energy 43.0 JInstrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
@Thickness 3.17 mm
ASTM D648
Vicat Softening Point 127 °CRate B; ISO 306
UL RTI, Electrical 85.0 °C
@Thickness 1.57 mm
UL RTI, Mechanical with Impact 85.0 °C
@Thickness 1.57 mm
UL RTI, Mechanical without Impact 85.0 °C
@Thickness 1.57 mm
Flammability, UL94 HB
@Thickness 1.67 mm
 HB
@Thickness 1.67 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Asahi Kasei Stylac™ 518 ABS Polymer, Flame Retardant: Halogen
A. Schulman Diamond ABSPC 8901P ABS/PC Plating Grade, High Impact
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced

PB1B03 / 26396

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.