MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oxford Polymers PC 46 Unfilled Polycarbonate for Blow and Extrusion Molding
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Unfilled Polycarbonate for Blow and Extrusion Molding

Information provided by Oxford Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.15 %ASTM D570
Linear Mold Shrinkage 0.0060 cm/cmASTM D955
Melt Flow 5.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9500 psiASTM D638
Tensile Strength, Yield 9000 psiASTM D638
Elongation at Break 110 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
Tensile Modulus 345000 psiASTM D638
Flexural Strength 13.5 ksiASTM D790
Flexural Modulus 340 ksiASTM D790
Compressive Strength 12.5 ksiASTM D695
Izod Impact, Notched 15.0 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 280 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 270 °FASTM D648
Flammability, UL94 V-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 550 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding
Oxford Polymers PC 68 Unfilled Polycarbonate for Injection and Extrusion Molding
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding
Oxford Polymers PC 1518 Unfilled Polycarbonate for Injection Molding

POX00 / 55849

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.